Default Re: Questions about polishing stainless steel

The moulds are in very good condition with no dents or major marks, but they are over 30 years old so there are lots of scratches mostly fine that make the mould appear cloudy.

the results that i am getting are ok. the problems im having are probably due to inadequte sanding, ie: not removing all scratches left by a lower grit paper

these are a couple of pics i took that appear ok at first, but you can best see the scratches still left on the piece under the flash of the camera.

if anyone can give me any tips to improve the finish im all ears as im just a begginer