A flash or strike plate is when you plate something with a metal first, so that it can be plated with another metal. E.g. a nickel strike over steel, so it can be plated with acid copper.

A bright plate refers to the final plate you give something, that you want to appear bright.

Our regular copper plating system uses acid copper; you have to add battery acid to the solution.

Our Flash Copper is an alkaline system, meaning that it's safe for metals that would corrode in an acidic bath, such as Pot Metal.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote