View Single Post
  #4 (permalink)  
Old 09-14-2003, 03:55 PM
DALE DALE is offline
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default

I hate to discourage anyone but your printer efforts are not going to work.
The powder will form a solid layer over the ink,with no break lines in the powder you won,t be able to simply remove the powder covering the ink.
Also chemicals that affect powder attack it at the adhesion point starting from the powder edges and creeping underneath to release the bond. Let us not forget that you will need to get the xylene through the powder to remove the toner. My suggestion is to print onto the powder instead of under it or clear powder over the toner.