i thought they might rust if they were sand blasted or something lol. and yeah the bolts do rust. but the center peice kind of corrodes. its got a really high magnesium content. all of those racing wheels do, its for weight reasons. and that had like some kind of salt corrosion on it or something before i got them blasted. i was just wondering if something like that would happen to the rest of the rim? im not too sure.

if you look at this picture i took you can see there is like a line of rust on the alloy dish.. lol i guess theres a first for everything?