Default Re: Help!! Polishing Sandblasted Chrome.

after i had the rims sand blasted i sprayed them with rust treatment and let it soak in between where the face plate meets the rim all around the wheel. i cant take the face plate apart, and i cant take out the bolts either. i have had the bolts sand blasted clean of rust at the and i put rust treatment on them at the same time. and i will be painting the whole face of the wheel with laquor so i think that should be ok and stop it from oxidising again.

do you think that will be good enough?

its a long story why the wheels cant be pulled apart anymore. but trust me they absoulty cant. not if you want to put them back together again. lol