Default Cleaning help PLEASE????

I have been polishing for many years and have had parts plated after polishing, but my plater has always cleaned my plates for plating. Now I am set up to do my own plating but I cannot get the polishing compound to clean off of the plates. I used the degreaser that Caswell sent me with my kits and set it up per instructions but it simply does not clean the polishing compound.

Is their some chemical I can use to remove the polishing compound before I degrease and activate the parts for palting?

Thanks in advance.