there are varied methods and products for cleaning items.i personally use acetone in copious ammounts to clean and flush at the same time, using a lint free cloth as to not contaminate the item with fibres etc. the acetone will evaperate eventually.
i have used break cleaner in rattle can as well i have a new kitchen sink brush to get in the intricate areas but the brush isnt harsh to mark the item especially if i am polishing.

have you tried the search facility top right, keep trying typing the key words you think you will need to get your answers, there are a lot of threads out there, Chromo and banditperformance and the guys have given their help in a number of threads.