Copy Chrome can go directly over steel(not stainless steel) and brass.

Treat aluminum with the zincate solution first, then copy chrome.

Pot Metal needs to be plated with the pot metal primer plate or FLASH COPPER first.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote