Default Re: Questions about polishing stainless steel

Quote:
Originally Posted by garymcgowan View Post
"....what do you do different in the 2nd stage, as opposed to the 3rd stage. is it just the direction that you apply the workpiece against the wheel (cut/colour motion??


I think that is a mis-print. In stage 3 it should be done with a loose cotton wheel with green compound. In the second stage, first do a cut motion and then do a color motion.

Hope this helps.

Gary
Cool, i have been getting good results using that following combo

sisal/grey
spiral sewn/green
loose/green

-cheers