View Single Post
  #2 (permalink)  
Old 12-25-2007, 08:17 PM
CarWiz's Avatar
CarWiz CarWiz is offline
Experienced Metal Finisher
 
Join Date: Sep 2005
Location: South Texas
Posts: 363
CarWiz is an unknown quantity at this point
Default Re: Is there a chemical

There used to be chemical dips that worked very well but thanks to the eviron-mentals, they are no longer available. The hot-dip and/or wash tanks work pretty good but tend to be pricey for a small company or individual. Any of the amino soaps are about as good as you're going to get now days. The trick is to get the tank (and parts) HOT and use air agitation.

On the high-end, there's also ultrasonic cleaning tanks.