Default Re: Is there a chemical

Tng21,

I have an old copy of their printed catalog that has a multitude of information in it about the different types of aluminum and aluminum products. Well worth having, just for the information that is included in the catalog. Also some of their products have automotive uses.
I use their ALUMIPREP #33. Cleaning & Conditioning Chemical for Aluminum. Deep Cleans, Brightens, and Conditions...Removes Oxidation Corrosion...Chemically Etches Aluminum Surface...Prepares Aluminum for Painting...Prepares Aluminum for Welding.
You dilute one part ALUMIPREP with two to three parts water. I have a Quart bottle .946 liters.

John
Reply With Quote