Default Re: Huge Problem

i finally had white ano using caustic soda, and i was very sure this was a done deal, so i was trying to achieve what is shown on the pic but i ended up with the same problem as you, i think that my problem was the concentration of the caustic soda, also i think it was because my piece was pre anodized but what i dont understand is why the pre ano wasent completely removed, because the problem of the piece happened on the part i wasent completely ano clear.
Attached Thumbnails
huge-problem-dibujo2.jpg  huge-problem-dsc00859.jpg  