Default problems with yellow

i've some great results using yellow and yellow mix but recently im having trouble with them, its taking to long for the dye to penetrate the oxide im not doing anything diferent from what ive done before 1mil, 20 min in the colour mix. but now i have to dip the piece for about 1hour or two if i want the same result.