Blast cabinet on the way!!!
Realizing I need a blast cabinet, I counted my pennies and bought the best one I could afford. Is it the best cabinet...probably not, but it will get me going and was discounted a $100.00 off from Harbor Freight.
Cabinet details:
Dual side doors for long objects with a large front door for bulky items. Includes brass flow valve, two nozzles, air regulator, large particle separating screen and easy access clean out door. - Sturdy welded steel construction
- Rust resistant powder coat finish
- Extra bright, twin tube 18 watt fluorescent light
- Foot operated activation switch
- 25'' long reach rubber gloves
- Dust reclaimer outlet (dust reclaimer sold separately)
Nozzle sizes: 6 mm and 7 mm; Abrasive capacity: 15 lbs., Door opening dimensions: 19-3/4" W x 19-1/4" H (x2 side), 46" W x 13-11/16" H (front); Working area: 47-3/4" W x 24" D x 22-1/2" H; Viewing window dimensions: 22-1/2" W x 10-1/2" H, Air requirements: 50 to 125 PSI @ 12 CFM; Air inlet: 3/8"-18 NPT, Overall dimensions: 51" W x 36" D x 65-3/4" H, Shipping weight: 297 lbs.