Re: problems with yellow
If that's the case. I would heat the dye to 180* like you do when you first mix it. Stir it up real good. Then strain with a coffee filter. The dyes seem to start to come out of solution after sitting unused for a while. I do this to mine if I haven't used the color for a while and it works for me.
SS
|