Default Re: another outgassing question

This OGF additive says that it can be used with any powder. I wonder if this refers to any thermoset powders, or really any powder. I am coating these castings with a thermoplastic nylon. Does anyone know off hand if these are compatible? Perhaps I'll just get a sample and try it. It seems useful, even if not in this application.