Quick question about dyes.
View Single Post
#
2
(
permalink
)
01-04-2008, 12:19 AM
sswee
Moderator
Join Date: Nov 2004
Location: close to Austin, Texas
Posts: 1,212
Re: Quick question about dyes.
Should be although you may need to heat to 180* to put the pigments back into solution.
SS