Default Re: extreme newb question.....

cure temps are on the lables of the powders you buy
most powder cure at 350-380 for 20 minutes at part temp
part temp is when the part reaches 350 or the cure temp you start counting the 20 mins.

with hobby guns there is a rule that never fails , the 150 rule
coat the parts at 150 degress, it saves a lot of headaches.
but with a lamp that will be hard to do because the lamp only heats up the area in front of it .