duh, I can't believe I didn't realize it before, but I left these parts out overnight inbetween the acid bath and the dye baths because I didn't have enough time. Then the next day when I went to resume, there was what looked like a white-ish powder on the parts around the areas where the parts were hung. So I rinsed the powder off and continued business as usual but now I'm thinking I didn't rinse off all of that white-ish powder and it affected the dye process somehow.
|