Both kits give the same end results. The parts you are doing dictate which kit would be best.

Handfuls of nuts and bolts are plated more easily with an electroless system - no need to wire up each nut and bolt.

Larger parts are plated more easily, and cheaply, with an electroplating system.

Sounds like you'd be best off with the Copy Chrome Kit, and a mini electroless cobalt kit for your nuts and bolts (if you have a lot)
__________________
--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm

Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
Reply With Quote