Default Re: need help with surface prep

lye turns aluminium black and te muriatic acid turn it back in a very light grey color ready for ano, that is what im using, could you please describe your prep process, because im trying to use something that isnt as reactive as these because im working with 7075 and it isnt as resistant as other alloy so i've screwed a couple of tries.