i would probably do 120 through 600 grit the forget the sisal wheel , use a tight stiched wheel (the ones that have a row of stiches every half inch)and a higher speed tool . your biggest problem is notonly the tools .
if its your first part you polish , give yourself a chance to practice and everything will be ok.

mpierich ,you slipped in a french word in there (BEAUCOUPS) . are you french ?