Default Re: some thoughts on polishing stainless

the green contains chromium oxide its harder than emery which is why it cuts faster, using emery compound is a waste of time on SS. I get the best results after sanding then straight to green. I sometimes use yellow with a loose wheel, it improves the shine slightly......I also use the exact same process on Titanium with amazing results and minimal time.