Re: Pickle #4
It depends on you're use.
Steel activation = 8oz./gallon. For 200ml, this works out to about 0.422 ounces or about 12 grams.
Deoxidizing Copper and it's alloys - 8 to 16oz./gal.
Deoxidizing Zinc, Lead/solder - 4 to 8oz./gal.
Page 31 (Version 9) of the Caswell Plating Manual should help you.
|