Quote:
Originally Posted by FigureLLC View Post
the chrome is supposed to be clear coated, so either the chrome would end up semi-gloss or the semi-gloss black would end up gloss. and xtreme chrome is supposed to be fully cured before applying the clear. so without giving it too much thought, i'd think the order would be:

1) chrome base over entire part - full cure
2) gloss clear over entire part - partial cure till flow out
3) apply mask, shoot black
4) partial cure til flow out of black, remove mask
5) fully cure.

is that about right?
If I understand this right you're going to apply the masking to a partially cured clear?