Going to sound weird but is your circulating pump working ok?? Also 1.3 amps for 8 to 10 min.?? sounds like a long time to me, almost like your still burning the part. I polish up my parts first then degrease them soak them in my pickle soultion for 3 min. wash them off with distilled water then plate them. Is this what your doing??
|