Re: Do i need the deluxe anodizing kit for annoing pb guns?
I agree with Empire.
Also, for doing PB guns, you'll want to ano everything all at once. That means a much larger ano tank than just 5gal buckets.
I like the large rubermaid bins for tanks... get the largest they make for the ano tank, and 10gal bins for the dyes and such.
I suggest a 20 amp, 20 volt (minimum) CC/CV power source.
What you need form Caswell is:
Buffing wheels and compounds
De-ox/de-smut
SP degreaser
Dyes
High temp sealer
PS (if they have an appropriate size)
Chemicals you can buy locally:
Lacquer thinner
Battery acid
Distilled water
Lye
Additional apparatus to think about:
Bead blast cabinet
Large buffing stand
Reverse osmosis water purifier
racking system
heating/cooling system
open flame burners
Large canning pots
Small pump-up sprayer
__________________
Specializing in anodized graphics in Paintball guns.
|