The colors are cheap... it's the rest of the stuff that's going to cost ya. Caswell chemicals will run $100 or so.
The big hit is the PS. Plan on spending $250 minimum for that.
Apparatus will cost you another $100 or so (depending on if you have a camp stove or other means of heat).
Local chemicals will be another $50 or so.
I usually tell people to plan on spending $500 just to give it a try.
That doesn't include any metal prep equipment like blast cabinet or buffing.