Quote:
Originally Posted by 95gts
after the red coat, do you need a clear? Or does the red act like one? I think the red does, but like to make sure...this will be over polished metal and xtream chrome.
thanks.
|
Correct, no need to clear. Just to clarify, are you putting xtreme chrome on a polished part and then the candy red or are the polished and xtreme chrome two different parts?