Ceramic Coating Question?
I bought the Ceramic coating from Caswell to use on my headers. After applying the coating I baked them for 1 hour first at 500 degrees F and they looked like gray primer. I blasted them, reshot them and baked for 2 hours at 500 degrees and they still looked like gray primer.
My instructions say afterwards to burnish them with steel wool and put in a tumbler. Is this the final step or am I doing something wrong? I don't want them to look like shiny chrome but have a little shine. Is that what the steel wool does? Any help will be appreciated.
Thanks
Bill
|