Does anyone know of such an additive? I did a bit of searching on this forum and does not seem like this question has been brought up in the past.

I have a friend who wants some parts done in a color close to kawasaki green, looks similar to tropical green, from what I can see in the powders. He wants a wrinkle finish, however, and I have run into an issue finding this color as a wrinkle finish. I have done some google searching for an additive that will produce a wrinkle finish on a non-wrinkle powder but found nothing. In my searches I did notice that coating shops say they can wrinkle any finish, so it leads me to believe that there is such a thing out there.

I'm sure if all else fails, he could settle for a normal finish, but being able to wrinkle turf green or tropical green would be a plus.