problem with black dye
hi guys
i wonder if you can help me...i am very stupid and slow and new to this so please bear with me
i got all my full kit from carswell UK and im really happy with it
i use a small 9-14v ni-cad battery charger with varable amp output...it seems only to put out very low ampage but i only colour really small parts ...so maybe i would not want much bigger ampage?
temp here in scotland varys a lot from summer to winter...it may be a factor...ill need do some testing in that area
the problem---the black die on some parts seems to be dark and lush...but on others its more a dark blue
any ideas please let me know
best wishes
john
Last edited by johnnie7; 01-22-2008 at 05:08 PM.
Reason: misspelt
|