Quote:
Originally Posted by acidrain View Post
Get a good digital thermometer and for small amounts, just heat it in the microwave.
All of your chimicals are temperature sensitive:
de-smut 120F
SP degreaser 120F-140F
Ano bath 70F
Dye 140F
ok ill get on to that#

i dont use the supplyed degresser (maybe thats my problem?)...i normally turn the parts from solid and then polish them to a mirror shine ...
then i use a different degreeser..its more water based and leaves the parts quickly when rinsed and water beads dont form on the surface..so hopefully that ok??

the de smut is that the same as the deoxiser in my uk kit?


thanks for putting up with me

john