Default Re: tips for 2xxx series alloy?

thanks, that helps a lot.

EDIT - one more question, if I'm running 2xxx and 6xxx in the same batch can I just take out the 2xxx parts 3/4ths of the way through and adjust the amps accordingly? or do they need to be run separately.