Default Re: Can I brush plate Nickel onto Flash Copper?

You can brush plate nickel over the flash copper. The flash copper is alkaline, and can be plated as a strike over steel, pot metal etc. Acid copper can't go over these metals. Acid copper also can be built up very thick, used to electroform.
__________________
--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm

Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
Reply With Quote