Re: Colors and Color Wheel
Thanks for the help and hint guys.
Here's the colors I ordered.
Red Bordeaux 2R Anodizing Dye - 1 Pint
Yellow 4A Anodizing Dye - 1 Pint
Blue 4A Anodizing Dye - 1 Pint
Black HBL Anodizing Dye - 4oz
Fast Blue 2LWN Dye - 1 Pint
Gold S Anodizing Dye - 4oz
Color Wheel
Hopefully, I think these will let me make most other colors I will need to start with ( except the browns and some other darker colors)
Any hints, tips, etc. I should know about any of them. or just follow the standard directions of 140 for up to 20 minutes depending on shade I want.
(I already read about Ph and plan on setting it to caswells numbers)
Thanks again
Ron
|