View Single Post
  #1 (permalink)  
Old 01-26-2008, 10:19 AM
peter61 peter61 is offline
Amateur Metal Finisher
 
Join Date: Jun 2007
Location: Southern N.J.
Posts: 60
peter61 is on a distinguished road
Question Strange controller read out?

I fired up my controller for the 1st time,heres the display I got.On the the top PV read out I got EEE.E on the bottom SV readout I got 80.00.
When I pushed the set button I got PASS on the top PV read out and
000.0 on the bottom SV read out,with the 1st 0 flashing.I can change the numbers up and down but my oven will not fire up,any ideas?Thanks.

Peter
Reply With Quote