Thank you for the response. Nickel does not "tanish" as does brass but nickel does, I think the word is "oxidize". From what little I know, the sulfur content in the brass underneath the plating sort of "bubbles up" into the surface of the plating and then the sulfur chemically interacts with the oxygen in the air, thus creating this black stuff. I have been doing this removal work by hand and cannot get down to the metal only part of the metal pieces to be cleaned. Is there a wheel and compound that will remove the oxidation without removing any of the plating?