Default Re: Is There A Better Way To Remove Tarnish From Nickel?

phosphoric acid we use is about 10:1...just soak the part...can also use a buffer..tooth brush or anything to help the process..most will be removed on contact. warm or hot water works best.
phosphoric acid can be bought I beleive most hardware stores carry it..if not just look up chemicals in phone book...not that bad of a acid..if you get it on your skin its just itchy..don't get it in mouth, eyes or cuts...you will feel that lol