hello guys,
real sorry been a long time since i was on.
i will hunt out pics tonight and PM them to you.
i used my 2 inch air grinder with the velcro attachments, but the best i used was the dremel attachment i got from ebay with sticky backing, these made light work of the Ali, but they flew off easilly so i would get better glue etc to make them stick.
http://s42.photobucket.com/albums/e3...ndingdiscs.jpg
on and off it has took me around 8-9 man hours but if you go start to finish you can easilly shed a lot of hours off.
tng 21 has produced some fantastic work, he gives good advice and it just happens he lives a few miles away from me.
greaseless is the way ahead.also the Dremel and felt bobs were great.
regards,
brian