I have a question for you guys that have large ovens, but coat a multitude of different size and mass parts. Do you guys group your parts together according to size and mass during the cure process to get a full cure, and not a over cure? I mean if you put in a 20 pound chunk of aluminum in the oven, and 50 one pound chunks of steel, is this possible to cure at the same time? I have a 4'x4'x8' oven under construction right now, and just wondering how I should go about doing multiple different parts curing in it. If it is possible to do these at the same time, even though I know they take different times to heat up. I dont do mass parts of the same, I do one piece of this with one these kind of deals. Thanks