Thumbs up Re: Gun quality

This is the gun I use and the quality is very good for the price of the gun.Do a search on the forum to see the modifications to the gun that some guys have done and you will get great results.The only drawback with the gun for me is the minimal amount of powder one must use in the cup to get a nice cloud and no powder spurts.When doing large items like an mc frame it would be nice not to have to reload the cup.A big help also is a quality air pressure regulator at the gun and good air filtration/water seperation.Hopefully someday Caswell will come up with a pro gun with greater powder capacity at an affordable price.