We don't sell "Nickel Activator." It's a total rip off. It's automotive battery acid (sulfuric).

Add 2 parts acid to 1 part water
Let cool
Add another 1 part acid

Always add acid to water to avoid painful acid splashes.
__________________
--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm

Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
Reply With Quote