I just can't figure this out.
Well lately I have been getting random dullish spots on my parts.I just cant figure out why these spots are coming up.I ran multiple guns and never had this problem.Some one suggested it being dissolution?Idk I gotta figure it out tho.To help yall out a little I'm gonna list my steps.
Rinse parts off in paint thinner to remove lube and dirt.
Drop parts in lye to strip them.
Drop and scrub in rinse tank.
Buff parts to a nice shine.
Clean the compound off with soap and water between and after each buffing step.
Rack parts.
desmut the parts with desmut running around 100*
Run parts at 6apsf with tank between 65 and 72.
dump in rinse bucket.
straight to dye.
straight to sealer running at 180.
dump in water.
spray and wipe down with wd40.
Then either smile or frown.
Any idea why these spots come up?
|