Well, no problem I called and found they are infact 3lbs. I placed order today-and should receive shortly.

BTW I have some pitting on some hubs, I have sanded up to 600 grit-and it appeared to be gone...until I cut it with emery..
Is this something the greaseless will cut down?

Also, getting a super sisal bar, and wheel. Hoping that armed with greaseless, sisal wheel etc I can cut down on some time. I seem to have amount of work for now, but need to get it out and done right-or no $.