I didn't see anything about that @ Eastwood. anyhoo, I put a chrome base coat on & fully cured. then I put the black chrome on & let it bake for about 5 mins. after flow then pulled it out, let cool to around 100 deg. & sprayed the red then placed in the oven for a full cure. candies perform better if you cure them @ lower temps. for longer. if they hit the oven & the temp. is too high you get runs & sags.