Quote:
Originally Posted by manishnjain
Hi,
I have put up with a new plant of hard anodizing.
Please can u guide me in how to get the best results for my anodizing.
I am anodizing utensils but i am getting gray color anodized. I need jet black.
please guide me on the bellow question: -
1. What temperature shoult i anodize. 32*F
2. What should be my acid mixture(and how pure should be my acid). 1:1 or 1:2 by volume
3. What volts and amps should i anodize . Depends on if using CC or CV
4. What other chemicals can i us.
5. How should i do the sealing. Distilled water boil if for eating utensils
my tank size is:- length=13ft
Width= 3ft
Hight=3.5ft
please guide me.
thanking you
manish n jain
|
Your questions are out of the scope of this forum. The answers I gave are from my study of the anodizing procedure and are not from this forum. What you are asking about is Type III Hard anodizing. It is not a DIY project.
SS