Just to answer my own question: looks ike most of the matt finish was tarnish and residue that is coming off when I polish. The plating solution still has some juice left, as I tried plating the unplated areas using the brush method and it is working. At this point, the finish looks very nice, although I still have a way to go.
jeff
|