Quote:
Originally Posted by quadracer2cool4u View Post
Right now I'm using a 3" 2000 rpm velcro air sander and greasless compound to sand the parts before polishing. I'm intrested in buying some more sanders that would save me some time, I was thinking of buying another 3" velcro air sander that has 2800-16000 rpms and also comes with a 1 1/2 inch backing pad. I do alot of brake parts for atvs so somthing that can get into the nooks and cranys would be great. Do any of you use tublers? if so could you give some specs on them? What do you guys think is the best way to do paint stripping? should I just bead blast? Any input would be great!!!
Thanks and have a great day!!!
well not everyone does the same kind of parts or work with the same tools ,
but i think a 1/4 inch angle die grinder is very useful and if you can make or have someone do some adapters you can use it with cartrigre rolls , buffing wheels ( 3 inches and smaller) sanding pads and more.
stripping paint : sometimes easier and faster just to blast and sometimes i use paint stripper .