Default Candy Orange Powder Problems

I'm having some problems with a candy orange powder coat on a valve cover. I'd appreciate any help or comments. I'm using an almost chrome basecoat and curing it for 20 minutes at 400 degrees. It comes out perfect. I'm curing the candy orange for 15-20 minutes at 400 degrees also, except it comes out with light and dark speckles in it. Some areas are darker than others too. Does anybody know what may be causing this? Here are some pictures:

http://www.smpolishing.com/images/Po...orangesr20.JPG

http://www.smpolishing.com/images/Po...angesr20_2.JPG

http://www.smpolishing.com/images/Po...angesr20_3.JPG

I seem to have alot of trouble with metallic powders in general, regular colors always come out flawlessly. Also, does the anodize blue powder have to have a basecoat?
BTW, I'm using the base Caswell gun.
Thanks,
Matt
Reply With Quote